We also mentioned Guiyang carborundum wearable Floor construction will be affected from the temperature, the temperature is not high, nor low temperatures, below is mainly about the construction precautions at high temperatures, in fact the most important summer For summer, hot and dry, moisture evaporates quickly, then how should do?
1, when the summer heat construction, removal of floating pulp processes should be sufficiently in advance, mechanical polishing processes should quickly.
2, try to avoid the high temperature period of construction, can be used sooner or later bifurcated construction period, after using a variety of materials should be preceded by the Group B thoroughly stirred, then the proportion of the A, Part B into the mixing bucket Stir, then aging Pour quartz powder or powders, after uniformly stirred use (strict control note maturing time).
3, when the summer temperature is too high, the ingredients should be as soon as possible after use, generally within 30 minutes after use to prevent material condensation ,, artificial cooling measures, in order to ensure the relative humidity of the construction environment, can be artificial humidification of the construction site, construction After the site should ensure that there is someone to take care of, so as to avoid excessively high temperatures lead to Guiyang carborundum wearable Floor shrinkage cracks.
4, summer heat but will clear topcoat differential color, gray, blue appears may be greater, should be fully mixed before use.
After the final completion of construction, shall be affixed to plastic sheeting conservation. The direct impact on the construction of Guiyang epoxy floor coating effect, and high humidity also has a great impact on the appearance of the coating, especially to avoid construction at low temperature and humidity environment, it is generally less than 80% relative humidity can construction. Such coatings generally can be adjusted to accommodate different curing agent construction conditions. On the following temperature on the Guiyang epoxy floor of:
Note that this pre-construction ambient humidity conditions, partly because the substrate surface is easy to condensation, resulting in poor adhesion of the coating after the Road, on the other hand, after construction, before the film was dry surface is easy to condensation, causing surface defects In particular finish, in this case, water vapor easily amine curing agent to paint with, resulting in low surface gloss coating, hair spray, white, sticky, oil spots, low hardness and so on paint disease, greatly reduce surface decorative effect, causing serious rework. Special solvent-free paint, dry time is generally longer, immediately after the rain in the winter and spring of painted or lacquered evening are dangerous. But sometimes because the owner requested period, less prone to ideal weather conditions, then we need to take measures to improve the construction environment, such as the open air heating and dehumidifiers, etc.
Guiyang epoxy floor construction should be less than 80% relative humidity, in order to ensure the construction quality epoxy, and allowed to reach a certain age, we must recognize that all kinds of weather, all kinds of temperature on the Epoxy construction effects and hazards to avoid in the reach of the weather or temperature conditions of construction, so as to have a good construction effect.
我們也提到過貴陽金剛砂耐磨地坪的施工會受到來自溫度的影響,溫度高了不行,溫度低了也不行,下文主要講的是在高溫下的施工注意事項,其實最主要的是夏季,對于夏天,炎熱干燥,水分蒸發(fā)快,那么應(yīng)該怎么做呢?
1、夏季高溫施工時,去除浮漿工序應(yīng)適當提前,機械磨光工序應(yīng)迅速進行。
2、盡量避免高溫時段施工,可以采用早晚時段分叉施工,在使用各種材料前應(yīng)先將乙組充分攪拌后,再按比例將甲、乙組分倒入攪拌桶攪拌均勻,熟化后再倒入石英粉或粉料,均勻攪拌后使用(嚴格控制注意熟化時間)。
3、夏季溫度過高時,配料后應(yīng)盡快使用,一般再30分鐘內(nèi)使用完畢,以避免材料凝結(jié),、采用人工降溫措施、為保證施工環(huán)境的相對濕度,可采用人工對施工現(xiàn)場加濕、施工后的現(xiàn)場應(yīng)確保有專人照看,以免因溫度的過高導(dǎo)致貴陽金剛砂耐磨地坪干縮裂縫。
4、夏季高溫面涂更會清微分色,灰、藍色出現(xiàn)的可能更大,應(yīng)充分攪拌后再使用。
**施工完成后,應(yīng)加蓋塑料布養(yǎng)護。的好壞直接影響到貴陽環(huán)氧樹脂地坪的施工涂裝效果,高濕度也對涂層外觀有很大影響,特別要避免在低溫高濕的環(huán)境下施工,所以一般相對濕度小于80%時才可以施工。此類涂料一般可通過調(diào)整固化劑來適應(yīng)不同的施工條件。下面淺談溫度對貴陽環(huán)氧樹脂地坪的影響:
施工前注意環(huán)境濕度這一條件,一方面因為底材表面易結(jié)露,造成后道涂膜附著力不佳,另一方面,在施工后,漆膜未干前表面易結(jié)露,造成表面缺陷.特別是面漆,在此情況下,水汽易與漆中的胺固化劑反應(yīng),造成涂膜表面光澤低、發(fā)霧、發(fā)白、發(fā)粘、油點、硬度低等等漆病,大大降低表面裝飾效果,嚴重時造成返工。特別無溶劑面漆,表干時間一般較長,在涂漆后馬上下雨或在冬春季的傍晚涂漆都是有危險的。但有時因為業(yè)主要求工期,理想的天氣條件不易出現(xiàn),這時就需采取措施改善施工環(huán)境了,如開啟空調(diào)加溫和抽濕等。
貴陽環(huán)氧樹脂地坪的施工相對濕度應(yīng)小于80%,為了保證環(huán)氧地坪的施工質(zhì)量,讓其達到一定的使用年限,我們必須認識到各種天氣、各種溫度對環(huán)氧地坪施工的影響和危害,避免在達不到條件的天氣或溫度下施工,這樣才能有好的施工效果。